Sheet metal parts fail in two ways: the flat pattern does not close to the right outside dimension, or the design cannot physically be formed. Both are predictable, and both are cheaper to fix in CAD than on a press brake.
Start with the neutral axis
When a sheet bends, the outside surface stretches and the inside compresses. Somewhere in between is a layer that keeps its original length — the neutral axis. Its position, expressed as a fraction of the thickness from the inside face, is the K-factor. For cold-rolled steel it is typically 0.33–0.45 depending on the bend radius, and it is the single number that makes a flat pattern correct.
Bend allowance vs bend deduction
Both describe the same geometry from opposite directions:
- Bend allowance (BA) is the arc length of the neutral axis through the bend. Add it to the flat lengths of the two legs to get the blank.
- Bend deduction (BD) is what you subtract from the sum of the two outside dimensions. This is what most CAD and CAM systems use, and what the press-brake operator sees.
For a 90° bend with inside radius R, thickness T and K-factor K: BA = π/2 × (R + K×T) and BD = 2×(R + T) − BA. Use the tooling supplier's table for the radius you will actually run, not the one in the model.
Five design rules worth more than any formula
- Minimum flange length. Roughly 4× thickness plus the inside radius. Shorter than that and the punch cannot reach past the bend line without marking the part.
- Inside radius ≥ thickness. Bending tighter than 1×T cracks the outside fibre, especially in 5052 aluminium and 304 stainless. For hard tempers, allow 1.5–2×T.
- Hole-to-bend distance. At least 2.5× thickness plus radius from the bend line, or the hole distorts into an oval.
- Relief at the end of a bend. A notch or a small radius where a bend terminates stops the tear that otherwise runs into the flange.
- Consistent bend direction where possible. Every direction change is another setup. Bending all flanges up costs less than up-down-up.
Springback is not a rounding error
Steel springs back 1–2°, stainless up to 4°, aluminium 2–3°. The brake compensates by over-bending, but the compensation depends on the material temper and the tooling. On a 3 mm stainless part with a 90° bend, 2° of uncorrected springback moves a 100 mm flange by 3.5 mm — enough to miss a hole pattern entirely.
Tolerances to expect, not to demand
| Feature | Typical achievable | Notes |
|---|---|---|
| Laser cut profile | ±0.1 mm | Better on thin gauge, worse on 6 mm+ |
| Bend angle | ±1° | ±0.5° on a controlled setup |
| Bend position | ±0.2 mm | Measured to the bend line, not the outside |
| Hole to hole across bends | ±0.3 mm | Accumulates with each additional bend |
| Flatness after welding | 0.5 mm / 300 mm | Heat input is the variable; stress relief helps |
Swipe sideways to see all columns →
Don't forget what the finish does to a fit
Powder coating is 60–120 µm per face. On a 1.5 mm panel that is up to 15% of the thickness, and it will close a 0.2 mm clearance. Either mask the mating surfaces, or design the clearance for the coated dimension and say so on the drawing. Anodizing is thinner (10–25 µm) but grows into the hole as well as out of it.
The most expensive sheet metal part is the one that was designed as a solid model and never unfolded. If the flat pattern exists and closes, the part will fold.
We supply a DXF flat pattern with every quote so you can check the geometry before the tooling is set, and we will flag the flanges that cannot be formed on our brakes rather than discovering it at the machine.